Product Name Color Application Function Temprature Application Rate Tds/Msds
Cover Flux A1-f Pink Covering and drossing flux for molten aluminium alloys. 640°–750°C 0.5%–1.0% Request
Cover Flux 11a Pink Covering and drossing for molten aluminium alloys. 640°–750°C 0.5%–1.0% Request
Cover Flux A-4 Yellow Covering Flux for melting turning and borings,prevents oxidation and gas absorbtion. 640°–750°C 5%–10% Request
Cover Flux A-5 Reddish Covering flux for Reverberatory furnace. 640°–750°C 0.5%–1.0% Request
Cover Flux A-6 Off-white Cover flux for Al-Mg Alloys. 640°–750°C 2%–3% Request
Cover Flux A-8 White Furnace cleaning flux, removal of oxides build up from furnace walls 800°C Once a week Request
Cover Flux A-56 White Exothermic flux for bogie treatment, higher recovery of aluminium from dross. 720°–750°C 0.25% Request
Cover Flux A-224(50) Yellow Sodium free covering & drossing flux for Al-Mg Alloy 640°–750°C 0.5%–1.0% Request
Cover Flux A-224(1) White Injection flux to be used with flux feeder machine, removes oxides and other inclusion from bottom of the furnace, thus the removal is more effective. 640°–750°C 0.5%–1.0% Request

Product Name Color Application Function Temperature Application Rate Tds/Msds
GR 510 White Medium to low temperature exothermic drossing flux 690°C–720°C 0.1% - 0.3% Of the melt Request
GR-520 White Medium to low temperature mild exothermic drossing flux 700°C–720°C 0.1% - 0.3% Of the melt Request
GR-530 White Medium to low temperature moderate exothermic drossing flux 700°C–720°C 0.1% - 0.3% Of the melt Request
GR-540 White Medium to low temperature moderate exothermic drossing flux 730°C–760°C 0.1% - 0.3% Of the melt Request
GR A-1 L White High-performance Granular Flux For GDC/PDC Alloying Manufacturer 700°C–720°C 0.1% - 0.3% Of the melt Request
GR A-6512 White sodium free flux for Al-Mg alloys (Mg 2-10%). <700°C 0.1% - 0.3% Of the melt Request

Product Name Color Application Function Temperature Application Rate Tds/Msds
Modifier A-129 White Modifier for Al-Si eutectic alloys containing silicon 10%-13% 790°C-800°C 0.5% -1% of the melt Request
Modifier A-136 Blue Modifier for Al-Si eutectic alloys containing silicon 10%-13.5% 740°C-750°C 0.5% -1% of the melt Request
Modifier 36 Blue Modifier for Al-Si eutectic alloys containing silicon 10%-13.5% 700°C 0.5% -1% of the melt Request

Product Name Tablet Size in gm Application Function Color Temperature Application rate Tds/Msds
Grain Refiner A-113 P 50, 250, 500 Phosphorus-based grain refiner for hyper-eutectic alloy Redish 730°C-750°C 0.2%-0.4% Request
Grain Refiner A-113 M Powder Form Phosphorus-based grain refiner for hyper-eutectic alloy White 730°C-750°C 0.2%-0.4% Request
Grain Refiner A-2 B 500 Boron-based grain refiner for hypo-eutectic alloy White 720°C-750°C 0.1%-0.2% Request
Grain Refiner A-2 50 High Perfomance Titanium-Boron based grain refiner for hypo-eutectic alloy White 720°C-750°C 0.1%-0.2% Request
Grain Refiner A-4 H 50, 250, 500 Titanium-Boron based grain refiner for hypo-eutectic alloy White 720°C-750°C 0.15%-0.2% Request
Copper Phosphor PC-8 Granular / Ingot Copper-phosphor based grain refiner for Hyper-eutectic aluminum alloys Bronze 720°C-750°C - Request
Grain Refiner GR-1584 500 Sodium-free granular for cleaning & grain refinement of Al-Mg alloys White 730°C-750°C 0.2%-0.4% Request
Degasser Cum Grain Refiner DA-9 250, 500 Titanium based grain refiner for aluminum and aluminum alloys to refine the grain size Blue 720°C-750°C 0.2%-0.4% Request
Fluxes In Powder Form

Cover Flux A1-f

Color: Pink
Application Function: Covering and drossing flux for molten aluminium alloys.
Temprature : 640°–750°C
Application Rate: 0.5%–1.0%

Cover Flux 11a

Color: Pink
Application Function: Covering and drossing for molten aluminium alloys.
Temprature : 640°–750°C
Application Rate: 0.5%–1.0%

Cover Flux A-4

Color: Yellow
Application Function: Covering Flux for melting turning and borings,prevents oxidation and gas absorbtion.
Temprature : 640°–750°C
Application Rate: 5%–10%

Cover Flux A-5

Color: Reddish
Application Function: Covering flux for Reverberatory furnace.
Temprature : 640°–750°C
Application Rate: 0.5%–1.0%

Cover Flux A-6

Color: Off-white
Application Function: Cover flux for Al-Mg Alloys.
Temprature : 640°–750°C
Application Rate: 2%–3%

Cover Flux A-8

Color: White
Application Function: Furnace cleaning flux, removal of oxides build up from furnace walls
Temprature : 800°C
Application Rate: Once a week

Cover Flux A-56

Color: White
Application Function: Exothermic flux for bogie treatment, higher recovery of aluminium from dross.
Temprature : 720°–750°C
Application Rate: 0.25%

Cover Flux A-224(50)

Color: Yellow
Application Function: Sodium free covering & drossing flux for Al-Mg Alloy
Temprature : 640°–750°C
Application Rate: 0.5%–1.0%

Cover Flux A-224(1)

Color: White
Application Function: Injection flux to be used with flux feeder machine, removes oxides and other inclusion from bottom of the furnace, thus the removal is more effective.
Temprature : 640°–750°C
Application Rate: 0.5%–1.0%
Fluxes In Granular Form

GR 510

Color: White
Application Function: Medium to low temperature exothermic drossing flux
Temperature: 690°C–720°C
Application Rate: 0.1% - 0.3% Of the melt

GR-520

Color: White
Application Function: Medium to low temperature mild exothermic drossing flux
Temperature: 700°C–720°C
Application Rate: 0.1% - 0.3% Of the melt

GR-530

Color: White
Application Function: Medium to low temperature moderate exothermic drossing flux
Temperature: 700°C–720°C
Application Rate: 0.1% - 0.3% Of the melt

GR-540

Color: White
Application Function: Medium to low temperature moderate exothermic drossing flux
Temperature: 730°C–760°C
Application Rate: 0.1% - 0.3% Of the melt

GR A-1 L

Color: White
Application Function: High-performance Granular Flux For GDC/PDC Alloying Manufacturer
Temperature: 700°C–720°C
Application Rate: 0.1% - 0.3% Of the melt

GR A-6512

Color: White
Application Function: sodium free flux for Al-Mg alloys (Mg 2-10%).
Temperature: <700°C
Application Rate: 0.1% - 0.3% Of the melt
Modifier Flux

Modifier A-129

Color: White
Application Function: Modifier for Al-Si eutectic alloys containing silicon 10%-13%
Temperature: 790°C-800°C
Application Rate: 0.5% -1% of the melt

Modifier A-136

Color: Blue
Application Function: Modifier for Al-Si eutectic alloys containing silicon 10%-13.5%
Temperature: 740°C-750°C
Application Rate: 0.5% -1% of the melt

Modifier 36

Color: Blue
Application Function: Modifier for Al-Si eutectic alloys containing silicon 10%-13.5%
Temperature: 700°C
Application Rate: 0.5% -1% of the melt
Grain Refiner

Grain Refiner A-113 P

Tablet Size in gm: 50, 250, 500
Application Function: Phosphorus-based grain refiner for hyper-eutectic alloy
Color: Redish
Temperature: 730°C-750°C
Application rate: 0.2%-0.4%

Grain Refiner A-113 M

Tablet Size in gm: Powder Form
Application Function: Phosphorus-based grain refiner for hyper-eutectic alloy
Color: White
Temperature: 730°C-750°C
Application rate: 0.2%-0.4%

Grain Refiner A-2 B

Tablet Size in gm: 500
Application Function: Boron-based grain refiner for hypo-eutectic alloy
Color: White
Temperature: 720°C-750°C
Application rate: 0.1%-0.2%

Grain Refiner A-2

Tablet Size in gm: 50
Application Function: High Perfomance Titanium-Boron based grain refiner for hypo-eutectic alloy
Color: White
Temperature: 720°C-750°C
Application rate: 0.1%-0.2%

Grain Refiner A-4 H

Tablet Size in gm: 50, 250, 500
Application Function: Titanium-Boron based grain refiner for hypo-eutectic alloy
Color: White
Temperature: 720°C-750°C
Application rate: 0.15%-0.2%

Copper Phosphor PC-8

Tablet Size in gm: Granular / Ingot
Application Function: Copper-phosphor based grain refiner for Hyper-eutectic aluminum alloys
Color: Bronze
Temperature: 720°C-750°C

Grain Refiner GR-1584

Tablet Size in gm: 500
Application Function: Sodium-free granular for cleaning & grain refinement of Al-Mg alloys
Color: White
Temperature: 730°C-750°C
Application rate: 0.2%-0.4%

Degasser Cum Grain Refiner DA-9

Tablet Size in gm: 250, 500
Application Function: Titanium based grain refiner for aluminum and aluminum alloys to refine the grain size
Color: Blue
Temperature: 720°C-750°C
Application rate: 0.2%-0.4%

Need More Information?

Our technical team is available to provide detailed specifications, application guidelines, and customized master alloy solutions for your specific requirements.

Technical Data Sheets (TDS) & Material Safety Data Sheets (MSDS): Complete product specifications and safety information

Stay In Tune With Us

Contact Us

Connect with our Technical team through our website, phone, or email to explore your requirements.

Enquire Now

Have a question or need more details? Submit your inquiry now, and our team will get back to you with the information you need.

Delivery & Support

Need assistance? Reach out to our support team for prompt solutions and expert guidance.